Solar Cell Lab: I–V Curve and Efficiency
Vary sunlight, temperature and ideality factor and watch Isc, Voc, fill factor and maximum power point of a silicon cell.
Single-diode model: I = IL − I0[exp(qV/nkT) − 1], with IL ∝ irradiance and I0 rising steeply with temperature through the band gap (1.12 eV, silicon). Series and shunt resistance are ignored.
- Short-circuit current
- Open-circuit voltage
- Maximum power
- Fill factor
- Efficiency
Why do hot panels lose power?
Raise the temperature: Voc falls about 2 mV/°C per cell, while current rises only slightly, so power drops.
Link to the syllabus
The same photon energy E = hc/λ you measure in the LED lab must exceed the band gap for a photon to make an electron–hole pair.